I am a welding methods specialist and in need of Aluminium welding defects causes and remedies PPT
Reply
#2
A weld defect is any defect that compromises the usefulness of a weld. There are a variety of weld defects. Welding imperfections are classified according to ISO 6520, while their acceptable limits are specified in ISO 5817 and ISO 10042.


Aluminum welds often pose more problems than when working with steel since aluminum is a better heat conductor and a lower melting point. This combination exposes projects of welding of aluminum to problems such as burn and deformation.
In addition, unlike steel that can be soldered by a technique of drag or thrust, with the aluminum the gun can only be dragged (also called reverse technique).

The mold defect can be classified as follows:
  • Filling the related defect
  • Defect related to form
  • Thermal defect
  • Defect by appearance
Reply

Important Note..!

If you are not satisfied with above reply ,..Please

ASK HERE

So that we will collect data for you and will made reply to the request....OR try below "QUICK REPLY" box to add a reply to this page
Popular Searches: ppt on aluminium alloys, defects in casting ppt, defects and remedies ppt, weld defects and remedies, advantages and disadvantages of aluminium formwork, pollution remedies chavara, welding aluminium,

[-]
Quick Reply
Message
Type your reply to this message here.

Image Verification
Please enter the text contained within the image into the text box below it. This process is used to prevent automated spam bots.
Image Verification
(case insensitive)

Possibly Related Threads...
Thread Author Replies Views Last Post
  seminar report on 3d solar cells ppt paper presentation ppt seminars report on 3d solar cells ppt paper presentation ppt 5 43,276 15-04-2018, 08:39 AM
Last Post: Guest
  design and fabrication of welding slag cleaning machine 4 9,160 17-03-2018, 02:58 PM
Last Post: Guest
  laser beam welding ppt prashant..thakur 2 1,240 07-03-2018, 04:58 PM
Last Post: Guest
  ppt on design and implementation of intelligent campus security tracking system based on rfid and zigbee 7 16,095 09-02-2018, 02:20 PM
Last Post: udaya
Smile physics investigatory projects for class 12 cbse to set up a common base transistor circuit and to study its input and o 3 25,193 20-12-2017, 09:44 AM
Last Post: jaseela123d
  list of underwater welding schools in india 3 10,188 16-12-2017, 11:12 AM
Last Post: jaseela123d
  friction stir welding ppt pdf 1 871 05-04-2017, 02:19 PM
Last Post: jaseela123d
  design of flexible and rigid pavements using lime cement and flyash as stabilizing material 1 5,184 05-04-2017, 01:07 PM
Last Post: jaseela123d
Question scope and importance of study of recruitment and selection 1 5,486 30-03-2017, 05:01 PM
Last Post: jaseela123d
  friction welding by ansys 1 754 10-03-2017, 10:53 AM
Last Post: jaseela123d

Forum Jump: